Sunday, August 25, 2019

Re: Re: [MW:29994] WPS

Hi,

Your process is SMAW, which is QW-253, G no is Supplymentry essential variables and it becomes essential as per QW-403. (b) and (c) second paragraph clause.

If G1 vs G1, you cannot use as per above as A 105 is G2, where as still if your A 106 falls under grade C again this also falls under G2 (If A or B then G1) however A 105 is G2, hence irrelavant of impact or non impact G1 vs G2 combinations not ensured in WPS, so as per your approved WPS and as per above clauses, strictly you cannot use this current WPS for propsed material.

Thanks,
Muneeb 

From: Babur Khan
Date: 2019-08-25 19:25
Subject: Re: [MW:29993] WPS
Dear,
Please note that P number is same (P1 to P1). For group number A106 Gr. B Gr.1 and for A105 Gr. 2 ( Group Number only applicable for impact test requirements) so if there is no impact requirement you can use.

Muhammad Babur Khan
Sent from my iPhone

On 24 Aug 2019, at 5:41 PM, Vinay Thattey <vinay.thattey@gmail.com> wrote:

In my view , Yes 
API 5L X52 grade B is seamless Cs pipe .

On Fri, 23 Aug 2019 at 09:48, tuscano09@gmail.com <tuscano09@gmail.com> wrote:
dear all,

can I use the attached WPS for A106 pipe and A105 pipe fittings?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/08f4d0ee-d589-40b1-af5f-6889f66ce8a3%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OhHB0c%2BKq_u3kqo3zXefzCO9Dgz2UKXKePVYiqSgw-EnA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/80FEFC80-D2A4-4BC0-B196-92F74641A1A0%40gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...