Please note that P number is same (P1 to P1). For group number A106 Gr. B Gr.1 and for A105 Gr. 2 ( Group Number only applicable for impact test requirements) so if there is no impact requirement you can use.

Muhammad Babur Khan
Sent from my iPhone

On 24 Aug 2019, at 5:41 PM, Vinay Thattey <vinay.thattey@gmail.com> wrote:

In my view , Yes 
API 5L X52 grade B is seamless Cs pipe .

On Fri, 23 Aug 2019 at 09:48, tuscano09@gmail.com <tuscano09@gmail.com> wrote:
dear all,

can I use the attached WPS for A106 pipe and A105 pipe fittings?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/08f4d0ee-d589-40b1-af5f-6889f66ce8a3%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OhHB0c%2BKq_u3kqo3zXefzCO9Dgz2UKXKePVYiqSgw-EnA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...