I have a basic query on welding of finned tubes using high-frequency continuous resistance welding. 

Design Code of the component: ASME Sec VIII, Div. 1. 

Which is the applicable clause for qualification using ASME Sec IX?? Is it Table QW-263 ?? 

Kindly provide your feedback if there is any other criteria's or qualification requirements that are to be met.


Thanks.

Ruban Stanley S






--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7254192c-2b13-4249-ad62-4ac88f9ee683%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...