[MW:29981] Stainless steel gauging

Dear expert,

I need your technical advice:
Is gauging allowed for stainless steel material? 

If yes, is there any code as per asme which state this? 
Mind sharing? 

Best regards,
Pravin 
Singapore 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7dOrRyj71gGKshXYdKNUP%2BjbRFwr_VXu9Nf33YEf0mNGQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...