Tuesday, August 6, 2019

Re: [MW:29924] How many coupons needed for welders qualifications of welder from 2'' (OD:60.33 mm) SCH : 5.18 mm ) GTAW according to ASME SEC.IX.

Hi,
1 coupon for 2" OD pipe. (As per Sec.IX; QW303.2, Minimum length of coupon to be examined is 150mm)

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com



On Monday, August 5, 2019, 08:40:06 PM GMT+7, 'Raja kumarasamy' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear sirs,

How many coupons needed for welders qualifications of welder from 2'' (OD:60.33 mm) SCH : 5.18 mm ) GTAW according to ASME SEC.IX.




Regards 

 

Raja kumarasamy
Welding & Piping inspector
ADNOC Waste Heat Recovery Project
Ruwais, Abudhabi
UAE  Mobile:  +971-565495293
INDIA  Mobile:  +91-9487403889


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1308484406.1069275.1565010887764%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...