Sunday, August 25, 2019

Re: [MW:29995] How many coupons needed for welders qualifications of welder from 2'' (OD:60.33 mm) SCH : 5.18 mm ) GTAW according to ASME SEC.IX.

Have you observed any issue or failure with first coupen ?

On Mon, 5 Aug 2019 at 19:10, 'Raja kumarasamy' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear sirs,

How many coupons needed for welders qualifications of welder from 2'' (OD:60.33 mm) SCH : 5.18 mm ) GTAW according to ASME SEC.IX.




Regards 

 

Raja kumarasamy
Welding & Piping inspector
ADNOC Waste Heat Recovery Project
Ruwais, Abudhabi
UAE  Mobile:  +971-565495293
INDIA  Mobile:  +91-9487403889


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1308484406.1069275.1565010887764%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oj9TG2RHRqNbk6bP0z5YJcZ44Sg%3D4J%3DFk_p8xmUc-8Mjw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...