Dear experts
Please give me your valuable feedback with code reference.
A) One welder is qualified with dia 1" & above with GTAW(11mm)
B) Same welder also qualified with 2 7/8 & above with GTAW + SMAW (7.5 mm Gtaw + max to be welded smaw )
My question:
Can this welder welded any 2" joint which thickness is more than 11mm by using GTAW+SMAW process ??
Regards
Sangram
Sent from my iPhone
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/E4DEF482-CEE0-4A77-A796-AA166751B51E%40yahoo.com.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...