Dear 

We can use sa194 gr 7 nut in place of sa 194 gr 4 for low temperature carbon steel line. 

Regards 
A p gupta 


On Sat, 31 Aug 2019 at 0:23, Raghul
<raghul351991@gmail.com> wrote:
Welder made two coupon
1. Coupon with 6 mm thickness on the 1/2" pipe made by gtaw process
2.coupon with 15 mm thickness on 2-7/8" pipe made by gtaw+smaw process.

Is the welder qualify to weld on 1/2" pipe with gtaw+smaw process for qualified thickness?

Please explain

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4a02db6d-d531-4b87-a6be-76c6bfa924e1%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1059495175.589383.1567256979364%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...