Hi,
Yes. You can use for all fillet sizes on all base metal thickness. See below.
Thanks& Regards,
(Karthik)
Karthikeyan.S
QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282
E-mail : karthik6684@yahoo.com
On Wednesday, August 14, 2019, 10:23:45 AM GMT+7, Rejoy Thomas <rejoythomas90@gmail.com> wrote:
Dear all,
Can I weld a socket/fillet joint, where the thickness of base metal (pipe to half coupling) is less than 5mm, by using a WPS which is qualified for 5-50mm thickness (GTAW+SMAW, P1 to P1), since there is no groove/base metal thickness involved in fillet welds!! Kindly refer the clause during reply. Your earliest response would be highly appreciated!!
Thanks & Regards
Rejoy Thomas
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc278%2BDqB-e2PgNcmT0VjBtDQmjnHuuvUPoNbJipaMue8%2BLg%40mail.gmail.com.
Comments