Saturday, August 24, 2019

Re: [MW:29989] WPS

Hi Gents,
for material covered ,  make sure also thickness with in limits of WPS .

regards
Elsahhar 

On Fri, Aug 23, 2019 at 7:18 AM tuscano09@gmail.com <tuscano09@gmail.com> wrote:
dear all,

can I use the attached WPS for A106 pipe and A105 pipe fittings?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/08f4d0ee-d589-40b1-af5f-6889f66ce8a3%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADGm7%3DzC-k373G843rXBC7SBd-t1K8n901mq5ncd1_%3DcNYaaUA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...