The technical comparison can be found in this part of the code that I mention, it is in detail each of these tests and you can draw your own conclusions.

El vie., 19 oct. 2018 a las 10:50, muneebslsa@gmail.com (<muneebslsa@gmail.com>) escribió:
Hello Jose, 

I saw the same, but here the question is he want to waive pneumatic without any lieu, but UG-100 is on lieu for hydro to pnemuatic.

So in his case waiving pneumatic means obviuosly he wants to waive hydro too, as in his case standards itself are stringent for hydro.

We needs experts any previous lesson learnt? 

Regards

Muneeb.M



 
Date: 2018-10-19 15:43
Subject: Re: [MW:28445] pneumatic & hydro testing of pressure vessels
You can see ASME SECTION VIII DIV. 1: UG-99 and UG-100.

El vie., 19 de octubre de 2018 2:09 a.m., prashant pansare <prashant.pan17@gmail.com> escribió:
Dear All,

I have to conduct pneumatic test at 13 kg for 7 mtr. dia X 65 mtr. long pressure vessel.

As compressor required for such a huge test is hardly available, we are trying to convince client that pneumatic testing is risky as copmapred to hydro testing.

Kindly submit any evidences of accidents happened due to pneumatic testing of pressure vessels.

Also technical comparison of   pneumatic & hydro testing.

--
Thanks & Regds,

Prashant  Pansare
Cell no - 09987189854

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--

Ing. José Juan Jiménez Alejandro

ASME Independent Consultant 

and Technical Manager SSI-TPI

Cel. +52 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...