[MW:28506] RE: 28480] Welding of UNS31254

Hi,

Please see the attached document providing detailed information on UNS 31254 steel, including welding. Recommended consumables are highlighted. Usually Inconel 625(ER-NiCrMo3) is the preferred grade for this alloy. The other grades are recommended based on the design criteria.
You should check with reputed manufacturers, on the best recommendation.
I had dealt with Metrode products in the past. However there're other good manufacturers also.

Thanks.

P.Goswami.P.Eng, IWE.
Welding & Metallurgical Specialist

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Darshan Revdiwala
Sent: October 22, 2018 12:43 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:28480] Welding of UNS31254

Can anyone share practical experience for welding of UNS 31254 and consumables selection for Tig and SMAW process.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...