Re: [MW:28488] API 5CT L80

API 5CT is the manufacturingstandard for casing and tubing which always comes with threaded and coupled. So there is no welding involved during field installation. Hence this grades are not coming under section IX P numbers. There are some equivalent ASTM graded available like A519. Also I'm not sure the meaning of helical piles. It's helical welded pipes or something else. Because only seamless and erw pipes only produced under 5CT. 

If it's a structural work, then you can take the P number for A519 grade and prepare WPS inline with D1.1. 

On Tue, Oct 23, 2018 at 4:20 AM Mohammed Shaban <mhmshaban@gmail.com> wrote:
Thanks, Sam for your respond. the situation like that, we have helical piles ( tubular hollow section API 5CT L80 OD 244.9mm WT 12 mm) to be installed and then square base plate ASTM A36 thickness 20mm will be welded (fillet weld) on top of each pile and then the skids will be installed on the base plates.
Would you please, advise under which standard we can qualify WPS?

Appreciate your help.

On Mon, Oct 22, 2018 at 11:22 AM Sam SM <samuvel.masilamani@gmail.com> wrote:
API 5 CT L80 grade is an alloy steel used in casing and tubing pipes in drilling. In what way you are correlating this with AWS D1.1??

On Mon, Oct 22, 2018 at 9:27 AM Shaban <mhmshaban@gmail.com> wrote:
Dear Gents.

Would you please help, can we prepare WPS under AWS D1.1 to weld A36 to API 5CT L80.
API 5CT L80 not listed in D1.1 how will find the requirements.

Thanks in advance.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/QYILjkUZ-Lc/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...