[MW:28470] Re: Welding Electrodes

E8016-B2 is having increased Cr. compare to E8016-B1.
Please elobrate more, what is the reason for change & any code compliance applicable.

According to ASME section IX,  QW 404.12 its a supplementary essential variable and require re-qualification if you have CVN requirements.
 
Thanks & regards
Sandeep Kumar

On Thursday, October 18, 2018 at 2:50:27 PM UTC+3, mathafiza wrote:
Dear experts,

Can we use welding electrodes E8016-B2 instead of E8016-B1?

Regards,
Muhammad Hafiza

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...