Re: [MW:28527] Combined PQR

Rajesh, not for ASME, It is for AWS D1.1 what is being discussed here

On Mon, 29 Oct 2018 2:38 pm rajesh kaswala, <rajeshkasvala@gmail.com> wrote:
AS PER SEC. 9 

QW-306 Combination of Welding Processes
Each welder or welding operator shall be qualified
within the limits given in QW-301 for the specific welding process(es) he will be required to use in
production welding. A welder or welding operator
may be qualified by making tests with each individual
welding process in separate test coupons, or with a
combination of welding processes in a single test coupon.
Two or more welders or welding operators, each
using the same or a different welding process, may be
qualified in combination in a single test coupon. For
combination qualifications in a single test coupon, the
limits for thicknesses of deposited weld metal, and
bend and fillet testing are given in QW-452 and shall
be considered individually for each welder or welding
operator for each welding process or whenever there
is a change in an essential variable. A welder or welding
operator qualified in combination on a single test coupon
is qualified to weld in production using any of his
processes individually or in different combinations,
provided he welds within his limits of qualification
with each specific process.
Failure of any portion of a combination test in a
single test coupon constitutes failure of the entire
combination.

REGARD
RAJESH

On Sun, Oct 28, 2018 at 10:13 AM shakin thobias <shakinthobias@gmail.com> wrote:

D1. 1

On 26-Oct-2018 10:12 AM, "Nithin Joseph" <nithindsilva4u@gmail.com> wrote:
what is the welding code?

On Wed, Oct 24, 2018 at 2:11 PM shakin thobias <shakinthobias@gmail.com> wrote:
Dear experts

I need to qualify welders in Both FCAW and SMAW. can i do both qualification in same PQR. what are the parameters and range of qualification. qualify that welders to max 30 mm thickness range. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...