First of all for only welder qualification u need to qualify WPQ but u can also used to qualified WPS to make WPQ.
Base material Thickness is non essential variable for welder but weld deposited thickness is essential variable for welder so < 12 mm weld deposited thickness welder can do upto 2t weld deposit but more than t= 13 the qualification range is maximum.
For diameter less than 25 welder can do welding upto 2T.for 25 -75 mm again 2T but diameter more than 75mm qualified diameter is unlimited.
Base metal thickness is not an considerable for welder it's only for wps

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...