Dear All, 

For welding of ASTM A333 Gr.6 and related (Flanges and fittings) 

Please note the following:

1. You have to qualify the PQR with P1G1 to P1G2 only.
This will qualify all the combinations of group numbers.  (The ASME interpretation is attached for your reference.)

2. You can do the PQR on plate with P1G1 to P2G2

3. Position should be 3G. (In piping 5G or 6G can be followed) Refer QW-405.2

4. Minimum thickness limits are as per QW-403.6
(Suggestion: PQR 1 : 6mm plate to plate, GTAW; PQR 2: 6mm Plate to Plate: GTAW+SMAW or SMAW only; PQR 3: 10mm Plate to Plate GTAW+SMAW) these 3 PQR will give a range from 3mm to 16mm of base  material thickness.)

5. For Maximum thickness limits,if your construction code is ASME B 31.3, you have to limit your maximum qualified thickness as per Table 323.3.1

Regards,

Hareesh K V
+91-8547859202

On Fri, Aug 24, 2018, 7:28 PM Temburu Chiranjeevulu <chiru.qaqc@gmail.com> wrote:
Dear Experts,

1. WPS/PQR (P NO: 1, Group No-1 to P NO: 1, Group No-1 ) is available with contractor

2. Pipe material: ASTM A333 Gr.6 (P No: 1, Group No: 1)

     Flange/Fitting material: ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2)

     WPS/PQR ( P NO: 1, Group No-1 to P NO: 1, Group No-2 ) is not available with contractor 

3.  Charpy "V" notch test to be done

My query is 
 
Can I use WPS/PQR P NO-1, Group  NO-1 (PLATE) to P NO-1, Group NO-2 (PLATE)   for welding of  ASTM A333 Gr.6 (P No: 1, Group No: 1) to ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2) ?

Please give suggestions, Is it possible in accordance with ASME Section-IX  ?



CHIRANJEEVULU TEMBURU l Inspection Engineer-Mechanical I +918790956353.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...