API 5 CT L80 grade is an alloy steel used in casing and tubing pipes in drilling. In what way you are correlating this with AWS D1.1??

On Mon, Oct 22, 2018 at 9:27 AM Shaban <mhmshaban@gmail.com> wrote:
Dear Gents.

Would you please help, can we prepare WPS under AWS D1.1 to weld A36 to API 5CT L80.
API 5CT L80 not listed in D1.1 how will find the requirements.

Thanks in advance.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...