Monday, October 29, 2018

Re: [MW:28527] Combined PQR

Yes possible as per ix

On Mon, Oct 29, 2018, 4:08 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Is it possible to combine individualy qualified PQR to form single WPS 

On Mon, 29 Oct 2018 10:00 am shakin thobias, <shakinthobias@gmail.com> wrote:
As per reference Aws doesn't have provisions for qualifying multiple process in same plate. If any other methods to qualify?!!

On Sun, 28 Oct 2018, 12:35 pm Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
Code is D1.1, if possible ,pl give code ref for combination

On Fri, 26 Oct 2018 11:42 am prabir maji, <pk_maji@rediffmail.com> wrote:
Yes you can

Thanking you,


P.K.MAJI
Sr Surveyor,
BUREAU VERITAS (I) PVT LTD.,
e-mail:-prabir.maji@in.bureauveritas.com
NAGPUR,
www.bureauveritas.co.in
Mob:9422127912


From: shakin thobias <shakinthobias@gmail.com>
Sent: Wed, 24 Oct 2018 15:43:37
To: materials-welding@googlegroups.com
Subject: [MW:28493] Combined PQR
 
Dear experts
 
I need to qualify welders in Both FCAW and SMAW. can i do both qualification in same PQR. what are the parameters and range of qualification. qualify that welders to max 30 mm thickness range. 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...