[MW:28488] GTAW & FCAW - P92 Forging PQR Details

Dear Sirs ,

We are going to weld elbow to elbow of 16" Long Radius in production joint of material A182-F92, thk 60 mm, OD 406.4. 

As we could not able to order the Pipe material for PQR urgently, we are going to machine forging material A182 - F92, which is to be machined to Min. 30 mm Thk and OD of approx 200 mm, for safer side.

I also checked about welding consumables, for GTAW - Metrode 9CrWV & FCAW - SuperCore F92 from Metrode, but could not find the parameters.

As this is the 1st time, we are going to run this type of material for PQR, can you share your valuable info about the AWS Class, Bevel Prep, correct Welding Parameters, Preheat & Post Heat, PWHT requirements to control hardness, other the ASME II C code info.

Thanks and Regards,
Saravanan Sornam,
Suwon, Korea


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...