[MW:28523] Re: Using API 5LX65 FLG instead of A350 LF2 during qualification of A333 GR 6 P1G1 to P1G2



On Friday, 26 October 2018 10:12:27 UTC+4, Noor Osama wrote:
Dear Expert,

Is it possible to replace LTCS Flange A350 LF2 by Flange API 5L X65 during qualification of A333 GR 6 Pipes to A350 LF2 Flange.

--