[MW:28243] 6G WQT using 6GR WPS

Dear All,

My contractor would like to propose WQT for 6G position using 6GR WPS...My Question, could this proposal is valid as Per AWS D1.1 or ASME code?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35742] PQR- Chemical testing requirements

Good Day to all, Reference std: ASME SEX IX Material ASTM A106 Gr B Pipe Dia and thickness: 2" and 8.74 mm. Service Fluid: Normal fluid...