Thursday, September 13, 2018

Re: [MW:28272] Welding rod selection Chart(GTAW,SMAW)

Hi,
The attached file might be useful to you

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com



On Thursday, September 13, 2018, 2:18:37 PM GMT+7, Guru. Thilakar <guru.thilakar@gmail.com> wrote:


Dear Expert's, 
                          Kindly share me the welding consumable selection Chart of GTAW, SMAW for piping carbon steel, alloy steel & stainless steel. 
Dear Expert's give a guidelines for learner.



Regards,
Guru.G
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...