[MW:28278] Query for WPS P1 to P8 weld joint

Dear experts,

I have qualified PQR of {SA 516 Gr 60(P1 Gr 1) to (SA 240 TP 304L(P8 Gr1)} electrode used E309L(F no.-5&A no.8)(without PWHT ) condition.

Now i have job {(SA 516 Gr 60(P1 Gr 1) to (SA 240 TP 316L(P8 Gr 1)} 
& I have a electrode E309LMo(F no.-5&A no.8)(without PWHT ) condition. The above PQR suitable for to make the WPS for this process?.

 Regards.

DHAKSHNAMOORTHY.J



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...