Monday, September 17, 2018

Re: [MW:28294] Query for WPS P1 to P8 weld joint

YES

Στις Σάβ, 15 Σεπ 2018 στις 5:13 π.μ., ο/η JAYAPAL DHAKSHNAMOORTHY <jmoorthy191@gmail.com> έγραψε:
Dear experts,

I have qualified PQR of {SA 516 Gr 60(P1 Gr 1) to (SA 240 TP 304L(P8 Gr1)} electrode used E309L(F no.-5&A no.8)(without PWHT ) condition.

Now i have job {(SA 516 Gr 60(P1 Gr 1) to (SA 240 TP 316L(P8 Gr 1)} 
& I have a electrode E309LMo(F no.-5&A no.8)(without PWHT ) condition. The above PQR suitable for to make the WPS for this process?.

 Regards.

DHAKSHNAMOORTHY.J



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...