Sunday, September 23, 2018

[MW:28321] testing of inaccessible welded joints

Dear All.

Does anybody know there is NDT method that can inspected welded joints which are buried and not accessible?our concern is about finding of construction defects either surface and internal that have a good detect ability for linear ones particularly Transverse Crack.

Regards.
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...