Sunday, September 23, 2018

[MW:28321] Re: dimension for fillet weld

ASME Section IX is silent regarding your query.

On Friday, August 3, 2018 at 7:56:10 PM UTC+3, Souravbohray wrote:
what should be leg length and throat if  thickness is given in drawing only ?
how to decide it should be fillet of equal leg length or unequal leg length?
if the T joint ( fillet ) plates thickness are same or different than how do decide throat and leg size without help of drawing ?
please reply on the basis of asme sec 9 only.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...