Preferably use SS because of superior properties in terms of corrosion resistance & strength. I assume you are going to weld with 309L type consumables.

Otherwise use MS, weld with 309L, that what actually you are doing for the designed weld joint also.

Thanks & regards
Sandeep Kumar


On Thursday, September 27, 2018 at 1:55:59 PM UTC+3, Gopalakrishnan G wrote:
Dear experts
I want to do PQR for ss304L to is2062.my doubt is what material to be used for support to avoid distortion ? whether SS or MS ?.if I use MS for support any contamination will reflect in test piece?.kindly guide me.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...