[MW:28289] Conflict between ASME Section IX clause QW 404.12 & WQ 404.33

Dear all

Kindly give your views on the interpretation of ASME Section IX clause QW 404.12 & WQ 404.33 when SMAW & GMAW process are concerned.
My point, as both the variables are same for Change in Filler metal classification, QW 404.12 is a supplementary variable while the QW 404.33 is non-essential variables.

There are additional information in QW 404.12 compare to QW 404.33 however focused point i.e. ''A change in the filler metal classification within an SFA specification'' is same.

Thanks a lot.

Regards
Sandeep Kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...