Re: [MW:28340] Re: dimension for fillet weld

The information of the dimensions of the weld fillet if they are in ASME, but this information is not in Section IX, is in Section VIII Div. 1, which is the Construction Code and Dr. George Dilintas has already given the answer from the beginning.
Regards!.

El dom., 23 sept. 2018 a las 5:01, Lakshmankumar Bayyana (<lakshmankumar4@gmail.com>) escribió:
All the answers will not be shown in ASME SECTIONS
ASME is a reference guide.
Required leg length, throat thickness, equal or unequal leg lengths, staggered welding or continuous welding, pitch for stitch welds all will be decided and confirmed by designers based on the loadings and design calculations 
ASME code will guide you how to do?

Thanks and Regards 
Lakshman kumar. B 
+91 9440031459

Sent from my iPhone

On 23-Sep-2018, at 12:31 PM, sandeep kumar <sandeepdhiman63@gmail.com> wrote:

ASME Section IX is silent regarding your query.

On Friday, August 3, 2018 at 7:56:10 PM UTC+3, Souravbohray wrote:
what should be leg length and throat if  thickness is given in drawing only ?
how to decide it should be fillet of equal leg length or unequal leg length?
if the T joint ( fillet ) plates thickness are same or different than how do decide throat and leg size without help of drawing ?
please reply on the basis of asme sec 9 only.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--

Ing. José Juan Jiménez Alejandro

ASME Independent Consultant 

and Technical Manager SSI-TPI

Cel. +52 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...