Lets start with code practice, The throat size or leg length measurements is code specific i.e. EN or ISO code emphasis on throat (a) measurement while the AWS, ASME based on leg length criteria (that what you will generally found in the drawing or refeering AWS A2.4 or ISO 2553.. 
Now referring AWS D1.1, 
AWS D1.1 state that the minimum size fillet weld shall not be smaller than the size required to transmit the applied load ( clause 2.4.2.8) and table 5.7 gives the minimum size of fillet weld required based on base metal thickness involved. The weld measurement of size is the leg length.

while designing or working as per EN/ ISO codes the requirements of minimum and maximum fillet weld is 

Maximum size of fillet weld = 0.7t (where t is the plate thickness, smallest thickness in case of dissimilar thickness involved)
Minimum weld size is based on the application of the weld e.g. for railway the minimum fillet weld shall be 3 mm for aluminium and 2 mm for steel. Here the weld measurement is in terms of throat size. (above is as per EN 15085-3).
For structural welds, design based on DIN 18800-1 is 3 mm.

Above maximum size of fillet weld is based on shear loading criteria. according to which the maximum load that can be transferred by a fillet weld will be 0.7 times of plate thickness. a weld size beyond this will be waste of the resources.

Thanks & regards
Sandeep Kumar

On Friday, August 3, 2018 at 7:56:10 PM UTC+3, Souravbohray wrote:
what should be leg length and throat if  thickness is given in drawing only ?
how to decide it should be fillet of equal leg length or unequal leg length?
if the T joint ( fillet ) plates thickness are same or different than how do decide throat and leg size without help of drawing ?
please reply on the basis of asme sec 9 only.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...