Re: [MW:28269] Re: Pulse GMAW-Black spots observed- Argon +2%CO2

Face side

On Wed, Sep 12, 2018, 17:33 sandeep kumar <sandeepdhiman63@gmail.com> wrote:
its on face side or root side?


On Sunday, September 9, 2018 at 6:32:32 AM UTC+3, Hrushikesh Sangamnerkar wrote:
Dear expert,

Problem observed:
After welding Black spots are seen on weld. These black spots are not removed even after pickling & passivation.

MOC - SS 347
Filler metal - ER347
Dia. - 1.2mm
Gas used Argon + 2% CO2
Mode - Pulse
Flow rate - 10lpm

Note:

EDS analysis of weld doesn't show any carbon content.


Pl suggest some remedy by which these black spots can be avoided.


Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...