Wednesday, September 26, 2018

[MW:28341] PQR usage (SA 516 Gr. 70 to SA 36)

Dear All,

I Have a PQR for SA 516 Gr.70 (N) Plate with Charpy V-notch Test -20 degree C
Can we use this as a supportive PQR for SA 36 Welding Procedure Specification.
(No Impact Test)
Welding Position, Process , Consumables will be same.
No PWHT.

Thank You & Regards
Williams
Mechanical Engineer
P Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...