Hi,
The sample preparation for clad materials is always debatable and should mostly be addressed by end user specification. It should be dictated from the fact that service fluid is in touch with the final clad layer and considering the corrosion allowance. However you may check the entire cross section corrosion rates for your reference.
Thanks & Regards,
Harish
Harish
On Aug 29, 2018 12:10 PM, "Ali Asghari" <asgharialigl@gmail.com> wrote:
Dear All.Does anybody have any experiences or instruction for preparation of sample for G28?is there any requirement to remove clad material from surface and go through it or not?this question arises from this point that IGC comes from carbide & inter metallics that mostly possible in diluted area and also accepted corrosion rate is about 0.9 mm/year for 625. Now is it reasonable to prepare sample from interface or without removing of thickness and take it from surface?Regards.--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments