[MW:28213] Can I use WPS/PQR P NO-1, Group NO-1 (PLATE) to P NO-1, Group NO-2 (PLATE) for welding of ASTM A333 Gr.6 (P No: 1, Group No: 1) to ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2) ?

Dear Experts,

1. WPS/PQR (P NO: 1, Group No-1 to P NO: 1, Group No-1 ) is available with contractor

2. Pipe material: ASTM A333 Gr.6 (P No: 1, Group No: 1)

     Flange/Fitting material: ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2)

     WPS/PQR ( P NO: 1, Group No-1 to P NO: 1, Group No-2 ) is not available with contractor 

3.  Charpy "V" notch test to be done

My query is 
 
Can I use WPS/PQR P NO-1, Group  NO-1 (PLATE) to P NO-1, Group NO-2 (PLATE)   for welding of  ASTM A333 Gr.6 (P No: 1, Group No: 1) to ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2) ?

Please give suggestions, Is it possible in accordance with ASME Section-IX  ?



CHIRANJEEVULU TEMBURU l Inspection Engineer-Mechanical I +918790956353.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...