Dear

I Think you can refer SAES-A-004 PARA 7.18 / SAES-L-150 PARA 5.13, For the clarification of the sequence of welding and Coating related to pressure test. 

Thanks & Regards

PRADEEPKUMAR HORMIS

Mob: +966-58 16 20 710

Image result for QUALITY INSPECTION GIFS

 
 


 


On Mon, Aug 6, 2018 at 6:49 AM Nishanth Km <nishanthkm21@gmail.com> wrote:
Dear sir,

In standards H 201 not mentioned about hydro test requirement.

Please tell where this requirement is mentioned.

Regards,

Nishanth km

On Sun 5 Aug, 2018, 2:28 PM Mohamed Muneeb, <muneebslsa@gmail.com> wrote:
Yes it is an 100% mandatory after welding before hydro and fbe is as per the requirements of lineclass specification which can be only internal or both internal and external but externals can be done after hydro but internal should complete with random pipes and also Piping spools which has been welded, including bosses and direct attachments before hydro. 

This is normal practice inside and outside kingdom for saudi aramco projects. 

Check SAES H 201

Note: Before going for Fabrication of fbe, some spools cannot be internal coated because of feasibility, hence make sure you if you are fabricating spools with multiple elbows are any other strginet rolling we go with flange separator.

Check with the coating applicator for feasibility. 

Regards 

Muneeb 

On Sun, Aug 5, 2018, 1:35 PM Nishanth Km <nishanthkm21@gmail.com> wrote:
Dears ,

Is there any requirement that internal FBE coating to be done for weld joints before hydro testing?

Please reply .


Regards,

Nishanth km

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...