Saturday, August 25, 2018

Re: [MW:28221] Throat Thickness in welding between DIN-18800 part 1 & EN1993 part 1

ask client itself

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ASNT-Level II in PT,MT,RT & UT.
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sat, Aug 25, 2018 at 3:34 PM 'Bijay' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Experts

In one of my project I have facing problems in throat thickness of welding.
Our governing code for welding is DIN - 18800 part 1, but as per clients instruction we have to follow the EN 1993 part 1 for throat thickness.
I can't find anything regarding throat thickness. Please guide what to do ?
Thank you in advance.
 
With Regards

Bijay Kumar Choudhury
Mob +91 8980630973

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...