Sunday, August 5, 2018

[MW:28173] Interpretation: IX-13-01

Dear Experts, 

Please explain this interpretation, it will be very helpful for me..

Interpretation:IX-13-01

Question: Does QW-403.6 apply when the HAZ isn't subject to impact testing such as when qualifying a P8 material.
 Reply: Yes

Why QW-403.6 still applies when there is no impact testing...

Regards..

--