[MW:28154] i am looking for acceptance criteria according to asme section ix for visual examination

i am looking for acceptance criteria according to asme section ix for visual examination  of cap hight, undercut, lack of fusion, undfill, arc stricke, penteration, root concavity which article of Asme will help me ....?

--