Dear experts,
We have copper tube as per BS EN 1057 of R290 hard material. While establishing brazing procedure for Lap joint, tensile strength results are 240 Mpa to 260 Mpa (fracture in parent metal). As per sec. IX, QB 153 "the specimen shall have a minimum tensile strength that is not less than the specified minimum tensile strength of the base metal ( 290 Mpa) in the annealed condition.
My question is acceptance crieteria of tensile strength as material is hard and after brazing ( somewhat Annealed), we have to refer same as base metal tensile strength or any relaxation for annealed criteria. Any reference of code if available it will help to clear BPS.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment