Dear Experts, 

Please help me out from resolving the issue of reduction of area percentage.  What is the effect of reduction of area percentage decreased in 12.9 grade bolts requirements is 44% and observed value is 20% in Tensile testing. Material is 12.9 high strength bolts referral code is ISO 898.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...