Greetings,

For your mentioned thickness need pwht. 

If you ask regardless to thickness for hf which is to be understood hydrogen service yes required but not necessarily for p no 1,but yes our client requires for p3, 4,5abc.

So its your clients requirements and his spec to be followed. 


Thanks 

Muneeb 


On Fri, Aug 3, 2018, 7:56 PM Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:
Dear expert,

Query:
 
Service: HF
MoC: SA 516 Gr 70
P No. - 1
Thickness - 40mm

Is PWHT specifically required for HF service?

Client has not mentioned anything about Lethal or Sour service.

Pl suggest.

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...