[MW:28198] Cracked on Welding Joint P91 to 50 Cr 50 Ni

Dear Expert,

The Cracking found on  welded P91 to 50 Cr 50 Ni with welding consumable E NiCrFe-3 

If anyone has the comment on this

Thanks ,

Best Regards,

Nguyen ANh Tuan

--