Dear Experts,
                     We have repair in Golden joint and it is successfully done. But now client is asking for penalty for this joint as it was a 5% RT line.
But as per my understanding as it is a Golden Joint ( a 100% RT joint), so no need of repair penalty. But I am not getting any code reference to it. Please help me to find any reference.

Thanks and Regards,

Bishwambhar Kumar
Ph:- +974-55311582


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...