Re: [MW:28196] Golden Joint Repair Penalty

In this case an additional NDT, say UT is advisable. Please discus with your client.

Best Regards,

Shashank C Vagal (Quality Adviser), (+91) 8082395502, 8779046302,

NEO METAL-ANALYST & NDT SERVICES

·       A-25, Geet Siddhi, Boradevadi, Moshi-Haveli, PCMC, Pune 412105

·      301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA

www.neometalanalystndt.com / enquiry@neometalanalystndt.com / nach_sam@yahoo.com




On Monday, 6 August, 2018, 9:19:22 AM IST, Bishwambhar Kumar <bishwambhar10@gmail.com> wrote:


Dear Experts,
                     We have repair in Golden joint and it is successfully done. But now client is asking for penalty for this joint as it was a 5% RT line.
But as per my understanding as it is a Golden Joint ( a 100% RT joint), so no need of repair penalty. But I am not getting any code reference to it. Please help me to find any reference.

Thanks and Regards,

Bishwambhar Kumar
Ph:- +974-55311582


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...