Re: [MW:24746] Effect in future of oxidation in root weld for SS304

Corrosion resistance will be affected.

On 30 Apr 2016 8:41 a.m., "LALIT VADADORIYA" <lalit.vadadoriya@gmail.com> wrote:
Dear sir,

What will be effect in Oxidation in SS 304 root weld.

please expain.

Regards

Lalit Vadadoriya
Dy.Manager(Inspection)
Engineers India Limited

Dahej Petrochemical Complex,
Dahej (Gujarat)
Mob.9725214705

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKjb_1%2B54DqiQKhH7R%2Bfws_san5BDHLasMYRMr1GcnpWZR1Ttw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B6Tn1LAox%3DP71NpdCU7T_DKrSL_ohq6h7%2Bt%2BCw8ySkPSDhE0w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...