Wednesday, April 20, 2016

[MW:24723] welding filler metal for SS321

Dear Experts

Refer to API582 table A-2 proposed filer to weld SS321 to SS321 is E347-XX/ER-347 but some manufacturers such as ESAB propose E/ER-308LSi to this base material (SS321 to SS321) operating temperature is +350 C,
would you please advise in this issue.

Regards,
H.Nikdin