One method of heat input control is often referred to as the "run of the rod" method or the run out length. This method uses the provisions of ASME Section IX QW-409.1(b)(2). Basically, you measure the length of weld and length of SMAW electrode(s) consumed that then is the basis for determining the minimum length of weld that must be deposited per length of electrode burned. See below for Code reference.
Enjoy - John
From: 'prem_nautiyal26' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: Wednesday, April 13, 2016 6:25 PM
To: materials-welding
Subject: Re: [MW:24682] Run-Out Length for SMAW Process
Hi
Refer ASME Sec IX 2015 edition.
There is No such terminology called run out length mentioned !
Please ask your client for code reference.
Regards
Prem Nautiyal
9769316004
Sent from Samsung Mobile
-------- Original message --------
From: Kurniatullah Sirajudin
Date:10/04/2016 12:30 AM (GMT-05:00)
To: Materials & Welding
Subject: [MW:24660] Run-Out Length for SMAW Process
Dear Expert,
A week ago, i received comment regarding welding for smaw process.
My client ask to me, run-out length for smaw process.
I don't know what is run-out length.
Please advise me
Thank you & Regards
Kurniatullah Sirajudin
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb9ef69c-8c36-42e8-b090-7dd6d32d8af3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/x4wy765uvcnprjyvpuhdiica.1460589900305%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

Comments