This is related with heat input.
What is your design calls?
Is impact testing is called in design drawing ?
If yes , qualify WPS with QW 409 supplementary essential variables
Here travel speed is related to run out length
On Sunday, April 10, 2016 at 2:25:34 PM UTC+5:30, Kurniatullah Sirajudin wrote:
-- What is your design calls?
Is impact testing is called in design drawing ?
If yes , qualify WPS with QW 409 supplementary essential variables
Here travel speed is related to run out length
On Sunday, April 10, 2016 at 2:25:34 PM UTC+5:30, Kurniatullah Sirajudin wrote:
Dear Expert,A week ago, i received comment regarding welding for smaw process.My client ask to me, run-out length for smaw process.I don't know what is run-out length.Please advise meThank you & RegardsKurniatullah Sirajudin
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/886017a1-3e92-40a1-81e9-3e917fd17de1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments