Skip to main content

Re: [MW:24663] High YS to Low YS

dear Munden

please refer trailing para extracted from ASME section IX. I hope this may help you

QW-200.3 To reduce the number of welding procedure
qualifications required, P‐Numbers are assigned to
base metals dependent on characteristics such as composition,
weldability, and mechanical properties, where this
can logically be done; and for steel and steel alloys
(Table QW/QB-422) Group Numbers are assigned additionally
to P‐Numbers. These Group Numbers classify
the metals within P‐Numbers for the purpose of procedure
qualification where notch‐toughness requirements are
specified. The assignments do not imply that base metals
may be indiscriminately substituted for a base metal
which was used in the qualification test without
consideration of the compatibility from the standpoint of
metallurgical properties, postweld heat treatment, design,
mechanical properties, and service requirements. Where
notch toughness is a consideration, it is presupposed that
the base metals meet the specific requirements.


Regards,

Vivek Pandey
QC Engineer


On Sun, Apr 10, 2016 at 9:12 AM, meisam shokri arfaei <meisamshokri@gmail.com> wrote:
The YS is not a concern by its own.

You have to refer to the reference standard/code and check the material grouping system and essential variables which may cause re-qualification.

Regards

On Sat, Apr 9, 2016 at 6:13 PM, mubeenaws <mubeenaws@gmail.com> wrote:

Good day all 
Please help me out by providing u r advise on below request. 

We have a qualified WPS with 75K YS material as per Sec-IX, can we use on material with 65K YS for welding? 

Please provide your feed back with reference clause. 

Thanks and Regards 
Munden


Sent from my Samsung device

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/rjpr5c1o0br8nc1ww9xs5w5r.1460209404507%40email.android.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ASNT NDT Level III
International Welding Engineer

Mob.:+98 912 1394023




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtu%2BfCqHBaEm7Cg14tRd0wCU0TUdOUQw1FAi5-watJiPMw%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANCwoYkNd5f0iYyDCFf%2B5MBzydAR-yLFgUwVb20-jbO3SzP6TQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...